CT grades from ISO 8062 and GB/T 6414 define as-cast tolerance ranges for investment casting. This guide explains CT4–CT8, compares them to GB/T 6414, and shows when machining is more economical than tightening as-cast limits.
CT Grades and GB/T 6414: The Basics
In investment casting, dimensional tolerances are standardized by ISO 8062 and its Chinese equivalent, GB/T 6414. The CT grade (Casting Tolerance grade) indicates the precision level: lower numbers mean tighter tolerances. For investment casting, typical achievable grades are CT4 to CT6, while CT7 and CT8 are looser and more common in sand casting. GB/T 6414 mirrors ISO 8062 but uses the same CT numbering; the key difference is that GB/T 6414 includes a table of tolerance values for each grade and nominal size range. For example, for a nominal dimension of 50 mm, CT4 allows ±0.20 mm, CT5 ±0.28 mm, CT6 ±0.40 mm, CT7 ±0.56 mm, and CT8 ±0.80 mm. These values scale with size: at 200 mm, CT5 is ±0.70 mm, CT6 ±1.0 mm, CT7 ±1.4 mm, CT8 ±2.0 mm. Investment casting can hold CT4–CT6 without special measures, but CT4 often requires wax injection tooling with tight process control and may still need selective machining.
What CT4–CT6 Really Mean in Production
CT4 is the tightest practical grade for investment casting. It requires high-quality wax patterns, minimal shell movement during firing, and controlled cooling. Achievable on small to medium parts, but for dimensions over 100 mm, maintaining CT4 becomes difficult and costly. CT5 is the workhorse grade: most investment casting suppliers quote CT5 as standard for critical dimensions. It balances precision and cost. CT6 is common for non-critical features, and CT7–CT8 are rarely specified for investment casting because they are too loose and waste the process capability. When a drawing calls out CT4 across all dimensions, expect higher tooling costs, slower cycle times, and more inspection. A better approach is to assign CT5 or CT6 to general dimensions and reserve CT4 only for functional features that cannot be machined later.
When to Specify Machining Instead of Tighter As-Cast Limits
Tightening as-cast tolerances beyond CT5 often costs more than simply machining the feature. For example, holding a ±0.10 mm tolerance on a 50 mm as-cast dimension may require 100% sorting and rework, while adding a machining allowance of 0.5–1.0 mm and cutting the surface on a CNC lathe or mill can achieve ±0.05 mm or better at lower total cost. The decision rule: if the required tolerance is tighter than CT5 for the given size, or if the feature is a mating surface, seal face, or bearing seat, specify machining. Also, if the as-cast surface finish (typically Ra 3.2–6.3 μm for investment casting) is not smooth enough, machining is needed. Use this checklist to decide:
- Tolerance tighter than CT5 for the nominal size? → Machine.
- Feature is a sealing, mating, or sliding surface? → Machine.
- Surface finish requirement below Ra 3.2 μm? → Machine.
- Dimension crosses a parting line or is affected by shell joint? → Machine.
- Annual volume high enough to justify hard tooling for as-cast? → Consider CT4 with process capability study.
- Prototype or low volume? → Machine from CT6 as-cast blanks.
Practical Tips for Specifying Tolerances on Drawings
On your casting drawing, avoid blanket tolerance notes like 'all dimensions ±0.1 mm'. Instead, use GB/T 6414 or ISO 8062 with a general CT grade (e.g., CT5) and then call out tighter tolerances only on critical features. Remember that CT grades apply to as-cast dimensions; if you add machining, the final tolerance is governed by the machining process, not the casting. Also, specify datum systems clearly because investment casting can have slight warp; referencing datums that are machined first ensures consistency. Finally, communicate with your supplier early: they can advise whether a CT4 request is realistic or if a minor design change (e.g., adding a rib) would allow CT5 and save cost.
Frequently Asked Questions
What is the difference between CT grades and GB/T 6414?
CT grades are the tolerance classes defined in ISO 8062 and GB/T 6414. GB/T 6414 is the Chinese standard that adopts the same CT numbering and tolerance values as ISO 8062, so they are technically equivalent. The main difference is that GB/T 6414 may include additional tables for wall thickness and draft angles.
Can investment casting achieve CT4 on all dimensions?
No. CT4 is achievable only on selected dimensions with tight process control, typically small features under 100 mm. For larger dimensions or across parting lines, CT5 or CT6 is more realistic. Specifying CT4 everywhere increases cost and may lead to high rejection rates.
When should I choose machining over tighter as-cast tolerances?
If the required tolerance is tighter than CT5 for the size, or if the feature is a mating or sealing surface, machining is usually more economical. Adding a machining allowance of 0.5–1.0 mm and cutting the surface gives better precision and finish than pushing as-cast limits.
Looking for a reliable casting supplier? Request a quote from Intercontinental Casting — our engineering team replies within one business day.